Glass+Er,Yb-glass+Cospinel bonding crystal crylink

Glass+Er,Yb:glass+Co:spinel Bonded Crystal Case (1)

Customer Demand Trade Name Specification/mm Remark 92 High-temperature bonding Overall length 8.2±0.1mm, cobalt spinel T0=93.5%. Er glass length 2.7mm. Determine the length of the white glass according to the total length. PR film adopted Coating see requirements below 92 High-temperature bonding S Overall length 7.6±0.1mm, cobalt spinel T0=94.5%. Er glass length 2.7mm. Determine the length of the white glass according to the total length. PR film adopted Coating see requirements below Processing index: The absorption coefficient of cobalt spinel substrate for bonding is 0.4 cm-1. According to this coefficient, the length of cobalt spinel is about 1.68mm when T0=93.5% and …

Glass+Er,Yb:glass+Co:spinel Bonded Crystal Case (1) Read More »

NdYAG+VYAG bonding crystal crylink

Nd:YAG+V:YAG bonded crystal case (1)

Customer Demand Trade name Specification/mm Remark Nd:YAG bonded with V:YAG 2.8*2.8*14.2mm Nd:YAG length:10mm,V:YAG length:4.2mm, T0=75%@1319nm) Processing index: Coating: Nd:YAG side(S1 light-colored face): R<1%@808±5nm&R>99.9%@1319±1nm&R<0.5%@1064±1nm ,AOI=0±5° V:YAG side(S2 Green face): R=85%±2%@1319±1nm&R<0.5%@1064±1nm ,AOI=0±5° Damage Threshold:>700MW/cm2@10ns,10Hz,1319nm Picture of Shipment

Scroll to Top